- Grades
- 60/70 and 85/100
- Softening Point (60/70)
- 49 to 56 °C
- Flash Point (60/70)
- Min 250 °C
- Colour
- Black
Black Oils
Applications
Road Construction
Paving-grade bitumen for national, state and city roads.
Hot-Mix Plants
Binder for asphalt mixed at hot-mix plants.
Two Grades
60/70 for most Indian paving; 85/100 where a softer grade is specified.
Test Report
Certificate of Analysis
Bitumen · Every Line with Its Test Method
Grade 60/70
| Test | Method | Limit |
|---|---|---|
| Specific Gravity at 25/25 °C | ASTM D 70 | 1.01 to 1.06 |
| Penetration at 25 °C | ASTM D 5 | 60 to 700.1 mm |
| Softening Point | ASTM D 36 | 49 to 56°C |
| Ductility at 25 °C | ASTM D 113 | Min 100cm |
| Loss on Heating | ASTM D 6 | Max 0.2% w |
| Drop in Penetration After Heating | ASTM D 6 and D 5 | Max 20% |
| Flash Point | ASTM D 92 | Min 250°C |
| Solubility in CS2 | ASTM D 4 | Min 99.5% w |
| Spot Test | AASHTO T 102 | Negative |
Limits are the specification the product is tested against.
Grade 85/100
| Test | Method | Limit |
|---|---|---|
| Specific Gravity at 25/25 °C | ASTM D 70 | 1.01 to 1.06 |
| Penetration at 25 °C | ASTM D 5 | 85 to 1000.1 mm |
| Softening Point | ASTM D 36 | 45 to 52°C |
| Ductility at 25 °C | ASTM D 113 | Min 100cm |
| Loss on Heating | ASTM D 6 | Max 0.5% w |
| Drop in Penetration After Heating | ASTM D 6 and D 5 | Max 20% |
| Flash Point | ASTM D 92 | Min 232°C |
| Solubility in CS2 | ASTM D 4 | Min 99.0% w |
| Spot Test | AASHTO T 102 | Negative |
Limits are the specification the product is tested against.
Where It Comes From
Imported from Gulf refineries for the western Indian market, where the company has been bringing in base oil and bitumen for over a decade.
Used For
Road construction and hot-mix plants. 60/70 for most Indian paving; 85/100 where a softer grade is specified.
Despatch
Drums or bulk. Rates on enquiry by grade and quantity.
Need a Rate on Bitumen?
A quantity and a delivery point get you a rate fastest.
Send an Enquiryor call +91 99250 08686